Wrinkle Formation

We are hot forming the spherical dome of R170 & Thk 7.5. Dome is having S.F. 60mm. We have taken blank dia.600mm. The major problem we are facing is heavy wrinkles during forming. We are carrying forming in 4 stages even the problem is occuring.Dome material is alloy steel.