Welded With E-7018 Electrode Without Proper Baking -What Is The Action?

Damped E-7018 electrode welded in piping at some joints. To ensure the weld quality, what is the best way?

I suggest, 1) Raise NCR. 2) All joints examined by RT as a corrective action.

Correct me if I'm wrong? or Please suggest any better way?